Atomic layer deposition of UV-absorbing ZnO films on SiO2 and TiO2 nanoparticles using a fluidized bed reactor

David M. King, Xinhua Liang, Casey S. Carney, Luis F. Hakim, Peng Li, Alan W. Weimer

Research output: Contribution to journalArticlepeer-review

103 Scopus citations

Abstract

Atomic layer deposition (ALD) was used to apply conformal, nanothick ZnO coatings on particle substrates using a fluidized bed reactor. Diethylzinc (DEZ) and water were used as precursors at 177°C. Observed growth rates were ca. 2.0 Å/cycle on primary particles as verified by HRTEM. ICP-AES and XPS were used to quantify Zn:substrate ratios. Layers of 6, 18, and 30 nm were deposited on 550 nm SiO2 spheres for UV blocking cosmetics particles. TiO2 nanoparticles were coated in the second part of this work by ZnO shells of 2, 5, and 10 nm thickness as novel inorganic sunscreen particles. The specific surface area of powders changed appropriately after nanothick film deposition using optimized conditions, signifying that high SA particles can be functionalized without agglomeration. The ZnO layers were polycrystalline as deposited and narrowing of the FWHM occurred upon annealing. Annealing the ZnO-TiO2 nanocomposite powder to 600°C caused the formation of zinc titanate (Zn2TiO4) in both oxygen-rich and oxygen-deficient environments. The non-ideal surface behavior of the DEZ precursor became problematic for the much longer times required for high surface area nanoparticle processing and results in Zn-rich films at this growth temperature. In situ mass spectrometry provides process control capability to functionalize bulk quantities of nano- and ultrafine particles without significant precursor waste or process overruns. ZnO overlayers can be efficiently deposited on the surfaces of primary particles using ALD processing in a scalable fluidized bed reactor.

Original languageEnglish
Pages (from-to)607-615
Number of pages9
JournalAdvanced Functional Materials
Volume18
Issue number4
DOIs
StatePublished - Feb 22 2008

Fingerprint

Dive into the research topics of 'Atomic layer deposition of UV-absorbing ZnO films on SiO2 and TiO2 nanoparticles using a fluidized bed reactor'. Together they form a unique fingerprint.